Open access

Oxidative Stability of Fats and Oils Measured by Differential Scanning Calorimetry for Food and Industrial Applications

Written By

M.D.A. Saldaña and S.I. Martínez-Monteagudo

Submitted: 20 January 2012 Published: 23 January 2013

DOI: 10.5772/54486

Chapter metrics overview

9,092 Chapter Downloads

View Full Metrics

1. Introduction

Fats and oils are important ingredients in the human diet for nutritional and sensory contributions. The terms fats and oils commonly refer to their phase being solid and liquid, respectively. In addition, lipids are the main ingredients to manufacture various products, such as soups, butter, ready to eat food, among others for the food industry and other products, such as lipstick, creams, etc, for the cosmetic and pharmaceutical industries. Most of these products use vegetable oils from seeds, beans, and nuts, which are important due to their high content in polyunsaturated fatty acids compared to animal fats. However, oxidation of unsaturated fatty acids is the main reaction responsible for the lipid degradation, which is related to the final quality of the product. Furthermore, lipids undergo oxidation, developing unpleasant taste, off flavour and undesirable changes in quality, decreasing the nutritional value of the product and compromising safety of the product that might even affect health and well-being.

In general, oxygen reacts with the double bonds present in lipids, following a free radical mechanism, known as autooxidation. This reaction is quite complex and depends on the lipid type used and the processing conditions. The use of thermal processes, such as frying, sterilization, hydrolysis, etc, accelerate the oxidation of lipids. Various different reactions during lipid oxidation occur simultaneously at different rates. These reactions release heat that can be measured using differential scanning calorimetry (DSC).

Oxidation temperatures and kinetic parameters obtained from DSC can be used to rank and classify lipids in terms of their oxidative stability. Therefore, the reproducibility of oxidation experiments is crucial to evaluate the oxidative stability of lipids using DSC since variables, such as pre-treatment and amount of sample, the heating protocol, among others, strongly influence the results. Other methods that assess the extent of oxidative deterioration are peroxide value (PV) that measures volumetrically the concentration of hydroperoxides, anisidine value (AV), spectrophotometric measurements in the UV region and gas chromatography (GC) analysis for volatile compounds [1-3]. Over the years, thousands of studies have focused on monitoring and evaluating the oxidation of lipids using the Rancimat method, PV, AV, spectrophotometric and GC analysis of fats and oils from various sources. However, it is beyond the scope of this chapter to provide a comprehensive listing of all research using those methods. Comprehensive reviews on the oxidative lipid deterioration using those methods are well discussed somewhere else [4-6].

Among all these methods that measure the extent of lipid oxidation, DSC is widely used as an analytical, diagnostic and research tool from which relevant information, such as onset temperature of oxidation (Ton), height, shape and position of peaks are obtained and used for subsequent kinetic calculations. Kinetic information of lipid oxidation has been reported for a number of lipid systems, such as soybean/anhydrous milk fat blends, unsaturated fatty acids (oleic, linoleic, and linolenic acids), saturated fatty acids (lauric, myristic, palmitic, and stearic acids), “natural” vegetable oils (canola, corn, cottonseed, and soybean oils) and genetically modified vegetable oils.

This chapter focuses on the principles of lipid oxidation, the use of DSC technique to evaluate lipid oxidation, and recent studies on oxidative stability of fats and oils for food and industrial applications, addressing the generation and analysis of DSC thermograms for kinetic studies, where a method to analyse DSC data is described in detail, as well as the interpretation of kinetic parameters obtained at isothermal and non-isothermal conditions. In addition, some results on oxidation kinetics of milk fat after the use of traditional and emerging technologies, such as enzymatic hydrolysis and pressure assisted thermal processing are discussed in detail. Finally, conclusions on lipid oxidation analysis by DSC are provided.

Advertisement

2. Fundamentals of lipid oxidation

Lipid oxidation is a free radical chain reaction that leads to the development of unpleasant flavour and taste, loss of nutrients and formation of toxic compounds [7, 8]. Consequently, the shelf life and the final use of any lipid depend on its resistance to oxidation or oxidative stability [9]. The term lipid oxidation usually refers to a three consecutive reactions or stages, known as initiation, propagation and termination (Figure 1). In the initiation stage, free radicals are formed through thermolysis, where the break of covalent bonds is induced by heat. In addition, free radicals can also be formed due to the presence of enzymes, light, metal ions (Ca2+ and Fe3+) and reactive oxygen species. A list of initiators of lipid oxidation and their standard reduction potentials are provided somewhere else [10]. Compounds that homolyze at relative low temperature (<100˚C) are important initiators of radical-based chain reactions. Unsaturated fatty acids are compounds that homolyze at lower temperatures compare to saturated fatty acids. The homolytic products of unsaturated fatty acids are hydroxyl radical (HO), alkyl radical (RO) and hydroperoxyl radical (HOO), which further reacts with triplet oxygen to form peroxyl radicals. Among the starters, hydroxyl radicals are mainly responsible for the initiation of lipid oxidation due to its strong tendency to acquire electrons [10]. These radical products that have high energy, bond to a hydrogen molecule from the lipid structure, forming hydroperoxides (primary oxidation products). The formation of hydroperoxides can be repeated several times, propagating the oxidation reactions. Conjugated fatty acids have more than one type of primary oxidation products and more than one oxidation pathway, as previously reported [11, 12]. A kinetic analysis on autoxidation of methyl-conjugated linoleate showed that monomeric and cyclic peroxides are the major primary oxidation products rather than hydroperoxides [12]. Consequently, addition by Diels Alder-type reaction was earlier suggested as a reaction mechanism.

The next oxidation stage is the propagation, which consists in the further degradation of hydroperoxides or any other primary oxidation product [1]. There are mainly two types of degradation products from hydroperoxides. First, hydroperoxides interact with double bonds to form monomeric degradation products, such as ketones. The reaction occurs through the reduction of the hydroperoxyl group to hydroxyl derivative. Second, low molecular weight products, that results from the cleavage of the hydroperoxide chain, form aldehydes, ketones, alcohols and hydrocarbons. These low molecular weight compounds are responsible for the rancid and off-flavour produced by oxidized fats [1-4]. Finally, hydroperoxides and primary oxidation products homolyze to form peroxyl or alkoxy radicals that further reacts to form stable dimer-like products. In addition, alcohols, and unsaturated fatty acids (secondary oxidation products) also lead to termination products. The resulting compounds form viscous materials through polymerization as the oxidation proceeds. These polymers are oil insoluble and represent the termination stage of oxidation [2, 15].

Figure 1.

Main lipid oxidation reactions.

Advertisement

3. Fundamentals on the use of DSC to study lipid oxidation

The oxidation mechanisms presented in Figure 1 is an oversimplification because lipids consist of a non-homogeneous mixture of fatty acids. For example, anhydrous milk fat (AMF) is composed of more than 400 fatty acids with extremely diverse chain lengths, position and number of unsaturations of their fatty acids [13, 14]. Consequently, several reactions occur simultaneously at different rates as the oxidation proceeds. Although several methods have been used to analyze and monitor lipid oxidation [1], the oxidation reactions cannot be measured by a single method due to their complexity. Some of the available methods allow quantifying one or more reaction products of the different oxidation stages. Methods, such as oxidative stability index (OSI) and peroxide value (PV) are officially accepted by the American of Analytical Communities (AOAC) [1-6], while other methods are routinely used, such as the Racimat, chemilominescent, and volumetric methods [16].

An important overlooked characteristic of the oxidation reactions of lipids is the exothermal effect as the oxidation occurs. The released heat from a particular reaction can be measured using DSC in either isothermal or non-isothermal mode. For DSC oxidation measurements, the heat released from the oxidized oil is compared to the heat flowing from an inert reference (empty pan) both heated at the same rate. When the oxidation of the sample occurs, the recorded heat shows a peak which area is proportional to the amount of heat released by the sample. Figure 2 shows an ideal thermogram for the non-isothermal oil oxidation with the three consecutive reaction stages of initiation, propagation and termination.

The heat released by the oxidized oil is recorded as the heat flow signal (y-axis) as a function of temperature (x-axis). The period of time where no change in the heat flow signal occurs is known as the induction time (Figure 2) that is exemplified at the beginning of the thermogram. An excellent review on the theory and application of induction time is provided elsewhere [17]. The length of the induction time is often considered as a measurement of oil stability. During this period, no chemical reaction occurs. At the point in

Figure 2.

Ideal thermogram of non-isothermal oil oxidation.

which the heat flow signal separates from the baseline (straight line) is considered to be the end of the induction time (arrow (1)). Arrow (1) also indicates the start of oxidation or initiation stage. This stage is short and can be theoretically interpreted as the reaction between the radical, formed during the induction time, and the unsaturated fatty acid. The products of this reaction are unstable hydroperoxides that further react propagating the oxidation. A sudden increase in the heat flow signal is related to the propagation stage. The blue dashed lines illustrate oxidation reactions that occur and cannot be detected by the DSC because they are less exothermal. Finally, arrow (2) illustrates the termination stage, where stable products are formed. The red line is the actual heat flow recorded by the DSC.

In the next section, a set of recommended guidelines and laboratory practices are reviewed for the good use and analysis of data using DSC.

Advertisement

4. Important considerations for measurement of lipid oxidation using DSC

Although DSC is a simple, convenient and fast technique to measure lipid oxidation, some recommended guidelines should be considered to obtain reliable and reproducible results. Among those guidelines are the pre-treatment and sample preparation, amount of sample used, heating protocol, gas flow rate, and interpretation of DSC thermograms.

Sample pre-treatment – a representative amount of lipid sample should be used for DSC oxidation measurements. The lipid should be melted at a temperature that ensures that its thermal memory is erased. The melting temperature for lipids is quite diverse, ranging from -25 to 80˚C. Melting temperatures of some vegetable oils are provided elsewhere [18]. In some lipid-based products, the pre-treatment of sample involves the fat extraction from the food matrix. For example, fat from commercial baby formulas was first extracted with chloroform [19], and then the fat was further dried under vacuum. Therefore, the behavior of these extracted fats might be different from the fat in the original matrix. In addition, a proper chemical description of any pre-treatment must be provided together with the thermal history.

Sample preparation – a liquid sample should be loaded into the DSC pan using a syringe or a Pasteur pipette. The lipid oxidation measured by DSC can be conducted in an open aluminum pan or in a hermetic sealed pan with a pinhole (Figure 3). The main difference between an open pan and a sealed pan with a pinhole is the diffusion of oxygen and the amount of oxygen that is in contact with the sample. This is because the thermal conductivity of the air is smaller than that of the metal of the pan. Indeed, numerical simulations showed that the energy transmitted to the sample comes from the plate, which transmits the heat to the pan [20].

A comparison of glycerol oxidation obtained in an open pan and a hermetic sealed pan with a pinhole was earlier reported [21]. For experiments conducted in an open pan, the maximum heat flow temperature of oxidation of glycerol was around 40˚C lower than those obtained with sealed pans. In an open pan, the vapor produced during lipid oxidation leaves the pan as it is formed. This is because the purge of oxygen acts as a carrier of the vapor. Consequently, part of the mass is lost before reaching the temperature at which the oxidation starts. On the other hand, in a sealed pan with a pinhole, the vapor produced cannot escape from the pan, remaining in the oil. This vapor increases the pressure inside the pan and elevates the oxidation temperature. Contradictory results were reported for the melting temperature of benzoic acid and vanillin obtained in an open pan and a sealed pan with a pinhole [22]. No significant differences were observed in the onset temperature (Ton) and the peak maximum temperature (Tp). Unfortunately, studies with a direct comparison between the types of pans (open and sealed with a pinhole) for oxidation of are scarce in the literature. Indeed, the international organization for standardization does not specify the types of pans for the determination of oxidation induction time [23]. Although hermetic sealed pans with a pinhole have an additional cost to each experimental run, their use avoids contamination of the DSC chamber.

Figure 3.

Illustrations of common DSC pans: (a) hermetically sealed pan with a pinhole, and (b) an open aluminium pan.

Sample size – the amount of sample has significant effect on the shape of the thermogram and reproducibility of the DSC oxidation experiments as it is related to heat transfer within the pan. Figure 4 illustrates the effect of the amount of sample in hermetic sealed pans with a pinhole. For the sample with an optimum sample thickness (Figure 4a), the oil is in contact with excess of oxygen, facilitating oxygen diffusion within the oil sample. An earlier study [7] recommended 1 mm of sample thickness (approximately 1.5 mg of oil) to yield consistent results in non-isothermal oil oxidation. Similarly, no changes on the DSC thermograms using samples between 1 to 4 mg were reported [24]. A ratio of 1:3 (oil:oxygen) not only avoids diffusional limitations [6, 7, 25] but also allows the vapor molecules formed during the oxidation reaction to rapidly escape from the pan [26]. This enhances the baseline and the resolution of the oxidation thermogram [27].

On the other hand, an excess of sample (Figure 4b) creates a temperature gradient within the sample, especially at high heating rates [27]. Also, the diffusion of oxygen is limited, which broader the DSC oxidation curves. This is illustrated in Figure 5 where samples of 3 and 13 mg of anhydrous milk fat (AMF) were oxidized at 12˚C/min from 100 to 250˚C. Interestingly, the Ton of oxidation is quite similar between samples (181.12 and 179.33˚C, respectively). But, the use of 13 mg of AMF leads to a broader and less resolved curve. The deviation of the heat flow signal from the vertical edge (broadening) is attributed to a longer time needed to oxidize a larger sample and the development of a temperature gradient within the sample. Another reason is that the probability of vapor molecules to escape from the pan through the pinhole is considerable reduced. Consequently, the peak maximum temperature shifts to a lower temperature because some of the vapor molecules react, accelerating the termination stage of oxidation.

Figure 4.

Illustration of (a) optimum sample size, and (b) excess sample size, in hermetic sealed pans with a pinhole.

Heating rate – this is one of the most important parameters to determine the oxidative stability and oxidation kinetics of lipids. Before the start of the heating rate, an equilibrium period between 3 and 5 min is recommended to enhance the baseline. At slow heating rates, primary oxidation products, such as hydroperoxides generated during the initial oxidation stage, react with excess of oxygen to form low molecular weight compounds (intermediate oxidation products), accelerating the degradation process. At fast heating rates, these intermediate products are lost through evaporation before they react with the lipid, shifting to a high value the threshold DSC signal [6, 9]. This phenomenon is the basis to calculate the kinetic parameters from a DSC thermogram [28]. However, it is important to highlight that the heating rate should not exceed 25˚C/min since the temperature of the sample is different from the furnace temperature, creating a temperature gradient which affects the oxidation kinetics [29]. An important overlooked consideration is the temperature range at which the oxidation study should be conducted. In general, the temperature range should start and end as far as possible from the Ton and Tp (approximately a difference of at least 50˚C).

Figure 5.

Effect of sample size on non-isothermal oxidation of anhydrous milk fat at 12˚C/min. Ton – onset temperature of oxidation; Tp – maximum heat flow temperature.

DSC mode – oxidation experiments can be conducted in either isothermal or non-isothermal mode. Both methods provide analytical information, such as the oxidation induction time in the case of isothermal measurements and the oxidation onset temperature in the case of non-isothermal measurements [28, 29]. Further comparisons on the kinetic studies conducted in either isothermal or non-isothermal mode are discussed in the following sections.

Advertisement

5. Analysis of DSC thermograms

5.1. Location of key parameters

The analysis and interpretation of the generated DSC spectra consist in identifying key parameters, such as the induction time, onset and peak maximum temperatures. These key parameters are manually obtained from the DSC spectra. The Ton is obtained extrapolating the tangent drawn on the steepest slope of Tp. This procedure is usually performed

Figure 6.

Anhydrous milk fat rich in conjugated linoleic acid oxidized at 15°C min-1. (a) Determination of the start temperature (Ts) (inlet), onset temperature (Ton) and maximum heat flow temperature (Tp), and (b) zoom on the first and second derivatives that precisely locates the Ts, Ton, and Tp

manually by the DSC operator, relying in the equipment software. Inherently, there is certain degree of uncertainty associated with this procedure. A method that accurately and unambiguously determines those key parameters from the DSC spectra was early proposed for lipid crystallization [30]. This method was first developed to calculate onset, offset, and peak maximum temperatures in crystallization of binary mixtures of different triacylglycerols. More recently, the same methodology was adapted to calculate the start, onset and peak maximum temperatures in non-isothermal oxidation of anhydrous milk fat [9]. Figure 6 exemplifies the location of the start, onset and peak maximum temperatures for anhydrous milk fat rich in conjugated linoleic acid oxidized at 15˚C/min in a hermetic sealed pan with a pinhole.

Once the DSC curves are generated, the error associated with the raw data is calculated through standard deviation. Then, the first and second derivatives are calculated. The error is obtained from the baseline, which in Figure 6 corresponds to the segment of 140 to 178˚C. This is essential since the signal variability can be misinterpreted as a thermal event. In this method, a true thermal event was considered when the heat flow signal is twice greater than the standard deviation of the baseline. This criterion is known as the departure value (inlet Figure 6a). To locate the start temperature of oxidation, three criteria were considered. Firstly, the first derivative of the signal shows an inflexion point between a maximum and a minimum point of the signal (arrow (1)). Secondly, the second derivative reaches a maximum point on the heat flow signal (arrow (2)). Finally, the heat flow signal should be greater than the departure value (inlet). Tp was obtained when the first derivative of the signal intersects with the x-axis (arrow (3)) and the second derivative reached a maximum point on the signal (arrow (4)). Ton was obtained extrapolating the tangent drawn on the steepest slope of Tp.

5.2. Iso-conversional method

In chemical reactions, the degree of conversion (0 ≤ α ≤ 1) or extent of reaction of a particular compound is defined by moles at a given time divided by the initial moles [29]. Similarly, α in thermal analysis is defined by the heat flow at a given time or temperature divided by the heat flow at time or temperature at which the maximum heat flow signal is reached. The heat flow from the DSC spectra is converted to α based on the initial (signalo) and final (signalf) heat flow signals, as shown in equation (1).

α=signalosignalsignalosignalfE1

At a given degree of conversion, the reaction kinetics is described by a single-step reaction that follows an Arrhenius type equation within a narrow range of temperature. Then, the overall kinetics [31-34] is the result of multiple single-step reactions in the form:

dαdt=A exp(EaRT) f(α)E2

where t is the time, A is the pre-exponential factor, Ea is the effective activation energy, T is the temperature, and f (α) is the reaction model. This procedure, known as iso-conversional or model-free method, is used to calculate kinetic triplet parameters (effective activation energy, Ea, pre-exponential factor, A and constant rate, k) in thermally stimulated reactions [29-34]. As known, reactions are the sequence of physical changes that can be measured by thermal techniques.

In non-isothermal oxidation of lipids, the consumption of oxygen can be neglected due to the large excess of oxygen generated by a constant flow rate (>25 mL/min). Such condition allows the formation of peroxides, being independently of the oxygen concentration, which also means that the autoxidation is a first order reaction [7, 9]. This is an essential assumption for the calculation of the kinetic triplet parameters (Ea, A, and k). A commonly used iso-conversional method is the Ozawa-Flynn-Wall method. Using this method, a set of data (Ts, Ton, and Tp) was obtained for constant heating rates (β= dT/dt) from which the kinetic parameters were calculated using the following equations:

logβ=a 1T+bE3

where β is the heating rate (K/min) and T is the temperature Ts, Ton, or Tp (K). By plotting log β against 1/T, the effective activation energy (Ea) and the pre-exponential factor (A) were determined directly from the slope and intercept according to:

a=0.4567 EaRE4
b=2.315+log(AEaT)E5

where a and b are the slope and intercept from equation (3), respectively, and R is the universal gas constant (8.31 J/mol K). Therefore, the effective activation energy (Ea) and the constant rate (k) are calculated from:

Ea=2.19 R dlogβ dT1E6
k=A exp(EaRT)E7

5.3. Induction time

As mentioned earlier, the period of time where no change in the heat flow signal occurs is known as the induction time and its length is considered as a measurement of lipid stability [17]. The determination of the induction period is routinely conducted to evaluate stability of oils, lubricants, biodiesel, and pharmaceutical products [34-38]. Unfortunately, no standard protocol for the determination of the oxidation induction time has been developed for lipids.

Figure 7a illustrates the standard protocol for determination of oxidation induction time (OIT). The polymer sample (15 mg) is rapidly heated under nitrogen atmosphere (≤ 20˚C/min) until it reaches the temperature that corresponds to time, t1, which is the starting point for OIT determination. At t1, the atmosphere is switched to oxygen and the sample is held at the same temperature until t2 is reached. The difference between t2 and t1 is the OIT. A disadvantage of this protocol is to find an adequate temperature for the isothermal stage. For example, the use of a low temperature might considerably increase the OIT while the use of a high temperature might oxidize the sample immediately, making difficult to obtain a reliable baseline. In tests conducted in 16 different laboratories, it was demonstrated that OIT is associated with a high degree of uncertainty. On the other hand, Figure 7b illustrates the experimental protocol for the determination of oxidation induction temperature (OIT*). In this case, the sample is continuously heated at a constant heat rate (for example, 12˚C/min) under oxygen atmosphere.

Figure 7.

Determination of oxidation induction time, OIT (a), and oxidation induction temperature, OIT* (b). Tm – melting temperature, t1 – start of the oxidation induction time, t2 – end of the oxidation induction time. Adapted from reference [35].

Advertisement

6. Kinetic studies of oxidation of fats and oils

Tables 1 and 2 summarize oxidation studies of fats and oils using DSC. Most of the isothermal studies were conducted between 80 and 180˚C with different flow rates varying from 10 to 100 mL/min. The amount of sample used also varied from 3 to 30 mg and most of these studies used open pans. The oxidation onset times were quite diverse (23-108 min) and therefore the Ea values ranged from 50 to 130 kJ/mol, depending mainly on the oil composition, temperature, and amount of sample. For the non-isothermal studies, the temperature ranged from 50 to 350˚C and the heating rate used ranged from 1 to 25˚C/min. The onset oxidation temperatures depended on the heating rate and oil composition.

6.1. Isothermal studies

For isothermal oxidation, the heat flow signal generated at constant temperature is plotted against time (Fig 7a). From these curves, the start of the oxidation (t1) and the end of the oxidation induction time (t2) are first located and then used for analysis [39].

Table 1 summarizes the isothermal oxidation studies of fats and oils, such as peanut, safflower seed, blackcurrant seed, rice bran, cotton seed, Buriti seed, passion fruit seed, sunflower seed, soybean, linseed, canola seed, coconut, grape seed, palm seed, and sesame seed. Earlier studies on isothermal oxidation were imprecise because the baselines obtained were highly unstable, making it difficult to obtain oxidation onset times [40, 41]. However, stable baselines were currently obtained in the isothermal oxidation of linoleic, linolenic, oleic, stearic, peanut, safflower and blackcurrant seed oils [42]. These oils were heated under argon flow. After thermal equilibrium was reached, the gas flow was switched to oxygen, allowing the oxidation to start. The temperature used to conduct the oxidation test should be far below the self-ignition temperature for fats and oils (~ 350˚C). Thus, the recorded thermal events are due to lipid oxidation rather than combustion. Using this approach, the obtained induction times were reproducible and highly influenced by the test temperature and sample composition. Attempting to validate the isothermal DSC oxidation, an earlier study [43] isothermally oxidized purpurea seed, rice bran and cotton seed oils using the DSC and the Rancimat methods. At each tested temperature, the DSC oxidation times were shorter than those obtained using the Rancimat method for the same oil. Despite these differences, the oxidation times were satisfactorily correlated with the Rancimat induction times. Similarly, longer induction times were obtained with the use of the Rancimat method for Buriti pulp seed oil, rubber seed oil and passion fruit seed oil [44]. In these studies, DSC rapidly reaches the threshold of the heat flow signal. This difference is attributed to the small sample used in DSC experiments, allowing a higher oil-oxygen ratio compared to the Rancimat method. Moreover, to oxidize the oil, DSC employs pure oxygen (99% purity) while the Rancimat method uses air (~21% of oxygen).

Figure 8.

LipidExperimental protocolOxidation induction times (OIT, min)Ref.
Linoleic, linolenic, peanut, oleic, stearic, safflower and blackcurrant seed- 80-160˚C
- 5 mg in an open pan
- Flow rate = 8.3 mL/min
-Argon flow to equilibrate
At 120˚C
- Olive = 108
- Blackcurrant = 95
- Corn = 78
- Peanut = 68
- Sunflower = 69
- Linseed = 50
- Safflower = 43
At 130˚C
- Olive = 105
- Blackcurrant = 50
- Corn = 50
- Peanut = 54
- Sunflower = 22
- Linseed = 21
- Safflower = 18
[42]
Rice, cotton seed and B. purpurea- 110, 120, 130 and 140˚C
- 5 mg in an open pan
- Flow rate = 50 mL/min
At 110˚C
- B. purpurea = 483
- Rice = 132
- Cotton = 172
At 120˚C
- B. purpurea = 269
- Rice = 72
- Cotton = 92
At 130˚C
- B. purpurea = 99
- Rice = 36
- Cotton = 42
At 140˚C
- B. purpurea = 48
- Rice = 18
- Cotton = 20
[43]
Buriti, rubber seed and passion fruit oil- 100, 110, 120, 130 and 140˚C
- 5 mg in an open pan
- Flow rate = 50 mL/min
100˚C
- Buriti = 116
- Rubber = 106
- Passion = 778
110˚C
- Buriti = 42
- Rubber = 51
- Passion = 369
120˚C
- Buriti = 23
- Rubber = 25
- Passion = 163
130˚C
- Buriti = 7.8
- Rubber = 7.5
- Passion = 66.5
140˚C
- Buriti = 3.3
- Rubber = 3.3
- Passion = 30.3
[44]
Rapeseed and sunflower - 120˚C
- 30 mg in a sealed pan
- Flow rate = 600 mL/min
- Rapeseed: OIT120˚C = 1.5-1.9 min
- Sunflower: OIT120˚C = 0.6-1.2 min
[45]
Linseed - 130˚C
- 5 mg in a sealed pan - Flow rate = 60 mL/min
- Linseed: OIT130˚C = 23.1
- Linseed + 0.05% of antioxidant blend = 25.1
- Linseed + 0.2% of antioxidant blend = 33.1
- Linseed + 0.01% Butylated hydroxyl anisole (BHA) = 24
- Linssed + 0.02% BHA = 30.1
[49]
LipidExperimental protocolKinetic parameters (Ea, kJ/mol; A min-1; k, min)Ref.
Rapeseed, soybean, corn and sunflower - 121 to 149˚C
- 3.5-6.5 mg in an open pan
- Flow rate = 100 mL/min
- Soybean: OIT121-150˚C = 11-2.9; Ea = 67.2; A= 2.7x107
- Rapeseed: OIT121-130˚C = 16.2-10.4; Ea = 71.9; A = 1.2x108
- Corn: OIT114-130˚C = 23-3; Ea = 98.6; A= 5.1x1011
- Sunflower: OIT106-130˚C = 11-2.8; Ea = 84.6; A= 1.4x1010
[47, 48]
Soybean, rapeseed, and sunflower oil- 110-150˚C.
- 3-4 mg in an open pan
- Flow rate = 100 mL/min
- Soybean: OIT110-150˚C = 139-11; Ea = 72.4; A= 6.3x107; k150˚C = 0.073
- Rapeseed: OIT110-150˚C = 122-14; Ea = 83.4; A= 1.6x109; k150˚C = 0.084
- Sunflower: OIT110-150˚C = 64-4.4; Ea = 86.2; A= 8.7x109; k150˚C = 0.201
[50]
Canola, coconut, corn, grapeseed, peanut, palm kernel, palm olein, safflower, sesame and soybean- 110-140˚C.
- 5 mg in an open pan
- Flow rate = 50 mL/min
- Canola: OIT110-140˚C = 259-37; Ea = 86; k128˚C = 0.016
- Coconut: OIT110-140˚C = 325-44; Ea = 86.9; k128˚C = 0.011
- Corn: OIT110-140˚C = 166-21.4; Ea = 88.1; k128˚C = 0.021
- Grape seed: OIT110-140˚C = 74-7.5; Ea = 99.9; k128˚C = 0.056
- Peanut: OIT110-140˚C = 127-12.3; Ea = 99.1; k128˚C = 0.025
- Palm kernel: OIT110-140˚C = 539-70; Ea = 89.4; k128˚C = 0.007
- Palm olein: OIT110-140˚C = 515-82; Ea = 79.9; k128˚C = 0.006
- Safflower: OIT110-140˚C = 88-8; Ea = 104.3; k128˚C = 0.055
- Sesame: OIT110-140˚C = 542-20; Ea = 88.8; k128˚C = 0.007
- Soybean: OIT110-140˚C = 124-20; Ea = 80.8; k128˚C = 0.029
[51, 52]
Soybean, rapeseed, corn and peanut oil- 108-162˚C.
- 2-5 mg in an open pan.
- Flow rate = 100 mL/min.
- Rapeseed: OIT130-150˚C = 33-11; Ea = 64.4
- Soybean: OIT138-162˚C = 8.9-2.3; Ea = 51.3
- Corn: OIT147-160˚C = 13.5-5.7; Ea = 77.5
- Palm: OIT108-121˚C = 24-6.5; Ea = 82.3
[53]
Lauric, myristic, palmitic, stearic acids and their ester- 155-180˚C.
- 5-8 mg in an open pan.
- Flow rate = 100 mL/min.
- Palmitic: Ea = 125.1 ± 11.2
- Ethyl palmitate: Ea = 126.6 ± 5.0
- Glycerol tripalmitate: Ea = 105.3 ± 7.7
- Stearic acid: Ea = 134.3 ± 12.0
- Ethyl stearate: Ea = 128.5 ± 2.6
- Glycerol tristearate: Ea = 102.5 ± 10.9
- Lauric acid: Ea = 97.3 ± 7.3
- Ethyl laurate: Ea = 127.3 ± 6.3
- Ethyl myristate: Ea = 117.1 ± 5.4
[54]
Blends of cocoa butter/cocoa butter fat like- 130, 140, 150, and 160˚C.
- 5 mg in an open pan.
- Flow rate = 100 mL/min.
Cocoa butter/cocoa butter fat like
- 100/0: Ea = 106.2; A = 5.6x1010; k160˚C = 0.008
- 90/10: Ea = 105.1; A = 4.4x1010; k160˚C = 0.009
- 80/20: Ea = 105.9; A = 6.7x1010; k160˚C = 0.011
- 70/30: Ea = 95.1; A = 3.9x109; k160˚C = 0.013
- 60/40: Ea = 99.5; A = 1.5x1010; k160˚C = 0.015
- 50/50: Ea = 104.4; A = 6.7x1010; k160˚C = 0.017
- 0/100: Ea = 120.5; A = 1.9x1013; k160˚C = 0.055
[55]

Table 1.

Summary of isothermal oxidation studies of lipids using differential scanning calorimetry

A comparative study of sunflower seed oil and rapeseed oil oxidation using DSC and volatile analysis showed that the ratio of hexanal/2-trans-nonenal linearly correlates with the onset heat flow signal of the DSC spectra [44]. In addition, a correlation between the peroxide values with the oxidation onset time was developed to monitor rapeseed oil oxidation [44]. Unfortunately, the correlation was valid only for oils with peroxide values lower than 30 mmol O2/kg oil. In other study, the experimental oxidation data obtained from electron spin spectroscopy was compared with the data obtained from DSC oxidation [46]. The onset oxidation times were highly correlated for different fat and oil blends. However, the obtained correlations were valid only at moderate temperatures of 60˚C, which considerably limits the applicability of electron spin spectroscopy for oxidation analysis.

An investigation of isothermal oxidation of oils (e.g. rapeseed, soybean, corn and sunflower oils) used onset time (ton) to rank the oxidized oils in terms of their oxidative stability [47]. The high maximum heat flow time (tp) value indicates that the oil is more stable. Although these relationships were statistically validated, a single parameter to evaluate the oxidative stability can lead to overestimation of the oxidative stability. In the same study, the authors considered tp to be proportional to the rate of oxidation, which might not be valid. Indeed, peroxide value determinations showed that tp represents the oxidation termination stage while ton is associated with the rate of initiation [48]. Furthermore, the addition of antioxidants prolongs only ton while tp values were minimally affected [48]. The same behavior was also observed in the isothermal oxidation of linseed oil with the use of antioxidants [49]. The addition of BHA (butylated hydroxyl anisole) and a mixture of antioxidants (tocopherol, ascorbyl palmitate, citric acid and ascorbic acid) prolonged the onset time at 130˚C. All these approaches provided information of great value for validation of the DSC isothermal oxidation. However, these equations are limited for a set of temperatures and specific oils (Table 1). Additional factors, such as degree of saturation, amount of free fatty acids, chain length and the presence of natural antioxidants were not considered.

Using the isothermal method, the sample is heated at a constant temperature and the released heat is recorded as a function of temperature. Such situation allows the identification of the maximum heat flow time (tm), which linearly correlates with the temperature [39,48, 49].

logtm=AT1+BE8

where A and B are regression parameters. Due to the excess of oxygen generated by a constant flow rate, the formation of peroxides is considered to be independent of the oxygen concentration, which also means that the autoxidation is a first order reaction [48, 49]. This is an essential assumption for the calculation of kinetic parameters, such as effective activation energy (Ea), pre-exponential factor (A), and reaction rate (k).

Ea=2.19Rdlog(tm)dT1E9

Equations 8 and 9 have been applied not only to obtain the maximum heat flow signal [47-49] but also to obtain the oxidation onset time. An attempt to correlate induction times and kinetic parameters of isothermally heated rapeseed, soybean and sunflower seed oils at different temperatures was proposed [50]. The authors correlated the oxidation induction times with the tested temperature using Arrhenius-like equations. The obtained kinetic parameters were comparable to those obtained by the Rancimat method. The onset time values of 12 different oils obtained by DSC were reduced by half of their previous values for every increase of 10˚C in the oxidation temperature [51]. These relationships were further used to obtain kinetic parameters of DSC oxidation [52]. The Ea values of rapeseed, soybean, corn and peanut oils were strongly influenced by the amount of saturated fatty acids [53]. The oxidation of saturated fatty acids (C12-C18) and their esters revealed that the Ea values (100-125 kJ/mol) were within the same range for all the tested oils [54]. This suggests that the isothermal oxidation is not influenced by the carbon chain length. Another important conclusion from this investigation [54] is that the start of oxidation is similar for fatty acids, their esters and triglycerides. The kinetic oxidation parameters of cocoa butter blends were obtained using the oxidation onset time [55]. The blends were oxidized from 130 to 160˚C in an open pan. Interestingly, the Ea and A values were slightly affected by the addition of saturated fatty acids. But, k values considerably changed with the amount of saturated fatty acids. Thus, k values can be used to rank the oxidative stability of cocoa butter blends. However, the use of k values to evaluate oxidative stability might be valid only at the temperature tested since changes in the reaction mechanisms can occur as a function of temperature.

6.2. Non-isothermal studies

For non-isothermal oxidation studies, two maximum heat flow peaks are commonly observed in the DSC spectra [56-59]. But, only the first peak is related to lipid oxidation. This was demonstrated in non-isothermal oxidation studies of corn and linseed oils with different peroxide values [57]. A decrease in the onset temperature was observed as the peroxide value increased. Contrary, the first and second peak temperatures were not affected by increasing the peroxide value. Consequently, the first peak can be related to hydroperoxides formation while the second peak can be due to further oxidation of peroxides. In an earlier study [58], the weight loss of lecithin during non-isothermal heating under nitrogen flow rate was analyzed. The thermogravimetric analysis showed that in the temperature range of the first peak only 4% of weight was lost but above that temperature, the weight loss considerably increased. Therefore, changes in the DSC signal within the range of the first peak temperature were attributed to oxidation and those changes above that temperature corresponded to thermal degradation rather than oxidation (Figure 8).

Figure 9.

Reaction mechanism proposed for lipid oxidation under non-isothermal conditions.

The proposed reactions in Figure 8 resemble to an autocatalytic reaction scheme. Indeed, computer simulated DSC oxidation curves using autocatalytic scheme fitted well the experimental data [56]. Similarly, the non-isothermal oxidation of mustard oil was best described by an autocatalytic reaction scheme [58]. Therefore, it was proposed that Ton is the most representative reference point of lipid oxidation under non-isothermal conditions. In addition, kinetic parameters calculated from Ton were comparable to those obtained at isothermal DSC conditions (Tables 1 and 2) [56-59]. Similarly, non-isothermal kinetics was used to evaluate the oxidative stability of commercial olive oil samples [59-62]. The obtained kinetic parameters were comparable to those obtained with the Rancimat method.

LipidExperimental protocolKinetics parameters (Ea, kJ/mol; A min-1; k, min)Ref.
Corn and linseed oil- 50-300˚C
- 5 mg in an open pan
- β = 5-20˚C/min
- Flow rate = 166 mL/min
- Corn: Ea = 69.5±9.7; A = 1.25x108
- Linseed: Ea = 132.7±8.8; A = 1.15x1016
Onset temperature
- Corn + 47 mmol O2/kg = 146˚C
- Corn + 70 mmol O2/kg = 142˚C
- Corn + 93 mmol O2/kg = 137˚C
- Corn + 136 mmol O2/kg = 137˚C
- Corn + 145 mmol O2/kg = 128˚C
- Corn + 158 mmol O2/kg = 127˚C
- Linseed + 31 mmol O2/kg = 144˚C
- Linseed + 119 mmol O2/kg = 131˚C
- Linseed + 180 mmol O2/kg = 129˚C
- Linseed + 252 mmol O2/kg = 125˚C
- Linseed + 349 mmol O2/kg = 117˚C
- Linseed + 383 mmol O2/kg = 121˚C
[56]
Linolenic acid and soy lecithin- 50-300˚C
- 5 mg in an open pan
- β = 2-20˚C/min
- Flow rate = 6600 mL/min
- Linolenic: Ea from Ton: 65±4; A = 2.3x107; k100˚C = 0.016
- Linolenic: Ea from Tp: 78.9±6.9; A = 9.9x107
- Lecithin: Ea from Ton: 97±8l; A = 2.4x1011; k100˚C = 0.001
- Linolenic: Ea from Tp: 141.4±4; A = 9.4x1015
[57]
Mustartd oil- 140-350˚C
- 3-5 mg in an open pan
- β = 2, 5, 7.5, 10, and 15˚C/min
- Flow rate = 100 mL/min
- From onset: Ea = 90.6; A = 3.4x109; k225˚C = 0.97
- From 1st peak: Ea = 88.5; A = 1.4x109; k225˚C = 0.90
- From 2nd peak: Ea = 84.6; A = 4.4x107; k225˚C = 1.12
[58]
Olive oil- 2-3 mg in an open pan
- β = 4, 5, 7.5, 10, 12.5, 15˚C/min
- Flow rate = 100 mL/min
- Ea calculated from Ton: 72-104; A = 3.31x108 -1.1x1012 ; k120˚C = 0.09-0.015[59]
Blends of soybean/AMF - 100 to 350˚C
- 5-15 mg in an open pan
- β = 2.5-12.5˚C/min
- Flow rate = 100 mL/min
Soybean/AMF
- 100/0: Ea = 93.5; A = 1.25.6x1010; k200˚C = 0.57
- 90/10: Ea = 59.5; A = 2.5x106; k200˚C = 0.68
- 80/20: Ea = 58.4; A = 2.1x106; k200˚C = 0.71
- 70/30: Ea = 64.5; A = 1.1x107; k200˚C = 0.80
- 60/40: Ea = 70.2; A = 5.2x107; k200˚C = 0.88
- 50/50: Ea = 73.2; A = 1.1x108; k200˚C = 0.95
- 40/60: Ea = 102.7; A = 2.6x1011; k200˚C = 1.18
- 30/70: Ea = 102.8; A = 2.7x1011; k200˚C = 1.20
- 20/80: Ea = 105.8; A = 5.3x1011; k200˚C = 1.26
- 10/90: Ea = 117.4; A = 1.4x1013; k200˚C = 1.55
- 0/100: Ea = 89.5; A = 8.4x109; k200˚C = 1.09
[62]
Oleic, erucic, linoleic, linolenic and their ethyl esters and glycerol trioleate and trilinoleate- Temperature = 50-300˚C
- 5 mg in an open pan
- β = 2-20˚C/min
- Flow rate = 600 mL/min
- Erucic: Ea = 89.6±4.4; A = 4.9 x1010; k90˚C = 0.006
- Oleic: Ea = 88.4±4.7; A = 1.0 x1011; k90˚C = 0.021
- Oleate: Ea = 95±4.7; A = 9.4 x1010; k90˚C = 0.002
- Trioleate: Ea = 91.8±13.3; A = 4.4 x1010; k90˚C = 0.002
- Linoleic: Ea = 72±2.9; A = 1.6 x109; k90˚C = 0.071
- Linoleate: Ea = 76.4±5; A = 2.4x109; k90˚C = 0.024
- Trilinoleate: Ea = 74.3±3; A = 9.6x108; k90˚C = 0.020
- Linolenic: Ea = 62.4±3.7; A = 2.6x108; k90˚C = 0.027
- Linolenate: Ea = 74.5±8.2; A = 4.2x109; k90˚C = 0.082
[63, 64]
AMF with low, medium and high CLA content - 100 to 350˚C
- 2 mg in an sealed pan
- β = 3, 6, 9, 12 and 15˚C/min
- Flow rate = 50 mL/min
- Low CLA: Ea = 146.5; A = 4.1x1014; k200˚C = 0.026
- Med CLA: Ea = 112.4; A = 3.6x1010; k200˚C = 0.014
- High CLA: Ea = 87.6; A = 6.3x107; k200˚C = 0.013
[9]
Cotton, corn, canola, safflower, high oleic safflower, high linoleic safflower, high oleic sunflower, soybean and sunflower- 1-1.5 mg in a sealed pan
- β = 1, 5, 10, 15 and 20˚C/min
- Cotton: Ea = 63.3; A = 9.2x106; k = 0.37
- Corn: Ea = 77.7; A = 2.4x108; k = 0.43
- Canola: Ea = 88.4; A = 7.6x109; k = 0.51
- Sufflower: Ea = 75.2; A = 1.8x108; k = 0.44
- High oleic sufflower: Ea = 88.7; A = 3.1x109; k = 0.48
- High linoleic sufflower: Ea = 73.5; A = 1.1x108 k = 0.42
- High oleic sunflower: Ea = 86.5; A = 1.8x109; k = 0.47
- Soybean: Ea = 79.6; A = 4.1x108; k = 0.44
- Sunflower: Ea = 63.8; A = 1.1x107; k = 0.38
[7]
Base oil lubricants- 0.5 mg in a sealed pan
- β = 5, 10 and 20˚C/min
- Flow rate = 100 mL/min
- Ea = 13.8-83.9 kJ/mol; k = 0.11-0.75 min-1.
[25]
Rapeseed, soybean, sunflower, lard and highly rancid oils- 100-360˚C
- 3-4 mg in an open pan
- β = 5-20˚C/min
- 166 mL/min
- Antioxidants: BHT, BHA and PG
- Rapeseed: Ea = 64-73; A = 7.4x105-4.4x106
- Soybean: Ea = 62-64; A = 6.1x105-7.1x105
- Sunflower: Ea = 60-62; A = 4.1x105-6.6x105
- Lard: Ea = 92-93; A = 3.5x108-2.7x108
[65]
Fat extracted from baby formulas- 3-4 mg
- β = 4, 6, 7.5, 10, 12.5, 15˚C/min
- Flow rate = 50 mL/min
- Ea = 80-106, A = 7.4x109-1.1x10-13; k120˚C = 0.079-0.122[19]
High oleic sunflower (HOS) and castor oil with blends of antioxidants- 100 to 250˚C
- 3-3.3 mg in an open pan
- β = 10˚C/min
- Flow rate = 10 mL/min
- Antioxidants (0.5-2 wt %): TOC, PG, AA and MBP
- HOS: OOT = 191˚C
- HOS + PG: OOT = 225-233˚C
- HOS + AA: OOT = 206˚C
- HOS + TOC: OOT = 190-214˚C
- HOS + MBP: OOT = 226-242˚C
- Castor: OOT = 197 ˚C
- Castor + PG: OOT = 233-242˚C
- Castor + AA: OOT = 208-212˚C
- Castor + TOC: OOT = 195-203˚C
- Castor + MBP: OOT = 212-234˚C
[66]
Linolenic acid (LNA) with different phenols- 50-300˚C
- 3-5 mg in an open pan
- β = 5, 10, 20, 40, 40 and 80˚C/min
- Flow rate = 250 mL/min
- LNA: Ea = 70.4; A = 5.6x109 min-1; k90˚C = 0.792
- 0.26 BHT/LNA: Ea = 73±3.7; A = 8.9x109; k90˚C = 0.541
- 0.82 BHT/LNA: Ea = 79.6±8.4; A = 2.4 x 1010; k90˚C = 0.17
- 1.51 BHT/LNA: Ea = 87±5.5; A = 2.0x1011; k90˚C = 0.134
- 3.0 BHT/LNA: Ea = 91.9±4.5; A = 6.5x1011; k90˚C = 0.091
- 4.0 BHT/LNA: Ea = 95.8±2.4; A = 2.1x1012; k90˚C = 0.049
[67]
LNA with BHT, olivetol and DHZ- 50-350˚C
- 5 mg in an open pan
- β = 2-20˚C/min
- Flow rate = 250 mL/min
- LNA: Ea = 69.8±7.8; A = 2.2x109
- 1.2-11.6 BHT/LNA: Ea = 82-141
- 1.1-8.2 DHZ/LNA: Ea = 88-187
- 1.1-5.6 Olivetal/LNA: Ea = 84-129
[68]
AA – ascorbic acid; TOC – tocopherol; MBP – methylenebis (2,6 ditert-butylphenol); PG – propyl gallate; BHT- Butylated hydroxytoluene, DHZ-dehydrozingerone, AMF-anhydrous milk fat, CLA-conjugated linoleic acid, OOT – oxidation onset temperature.

Table 2.

Summary of non-isothermal oxidation studies of lipids using differential scanning calorimetry

According to the Arrhenius principle, oil with a high Ea value oxidizes faster at high temperatures, while oil with a low Ea value oxidizes faster at low temperatures. Unfortunately, calculated values of Ea should not be used as a single parameter to rank the oxidative stability of lipid systems. This was exemplified in blends of soybean/anhydrous milk fat [63] that were non-isothermally oxidized. Interestingly, as the percentage of unsaturated fatty acids increased, the onset temperature of oxidation decreased and the only kinetic parameter that exhibited the same pattern was the constant rate of oxidation. The calculated Ea value is the cumulative effect of all the Ea values available in the system during oxidation, including intermediate compounds that have their own kinetic values. An equation representing the overall activation energy for autoxidation of lipids was earlier proposed [54, 56]. The overall effect included activation energies of initiation (Ei), propagation (Ep) and termination (Et) based on the classical rate equation for autoxidation of hydrocarbons.

Unfortunately, equation (10) has been applied to limited fatty acids (C12-C18) [56, 57] and correlations between other kinetic parameters and the initiation and termination activation energies are needed.

E=Ep+12Ei12EtE10

The non-isothermal oxidation of different fatty acids and their esters [56, 57] showed that the calculated Ea values are similar among the different tested samples, indicating that the oxidation does not occur on free or esterified carboxyl groups of fatty acids. The non-isothermal oxidation of anhydrous milk fat with different ratios of unsaturated/saturated fatty acids showed that the start temperature of oxidation shifted to lower values as the ratio increased [9]. More importantly, the kinetics parameters (Ea, A and k) calculated also decreased. The onset temperature of oxidation not only is affected by the amount of saturated fatty acids but also by the presence and abundance of aromatic compounds and their alkyl substitutions [7, 25]. Kinetic parameters obtained from different oils were compared with structural parameters obtained with NMR spectroscopy. Moreover, an increase in the methylene carbons of the fatty acid chains increased the oxidative stability while conjugated structures were rapidly oxidized.

The addition of antioxidants to enhance oxidative stability of oils can be evaluated using the DSC in non-isothermal mode. A novel approach based on DSC data, named protective factor (PF) was provided in the literature [65]. In this investigation, the oxidation of methyl esters derived from rapeseed and waste frying oil was monitored at different concentrations of BHT and pyrogallol (PG). The oxidation onset temperature asymptotically increased with the addition of BHT and PG, without finding an optimum antioxidant concentration. In addition, the increase in the heating rate might change the reaction mechanisms in which antioxidants can capture free radicals, making difficult to compare their effectiveness. Therefore, the protective factor concept [65] was developed according to:

Protective factor (PF)= onset temperature of oil with antioxidantonset temperature of oil without antioxidantE11

Values of PF lower than 1 means that the antioxidant has a pro-oxidant effect. On the other hand, PF values greater than one can be considered as a measurement of antioxidant effectiveness. Another important factor is the physical stability of the antioxidants. In a comparative study [65, 68], the addition of BHT, BHA and PG was evaluated in rapeseed, soybean, sunflower and lard oils. BHA and BHT were not effective antioxidants due to their volatility. These antioxidants escaped from the heated oil before they can react to neutralize free radicals. An optimum antioxidant concentration was found for BHT (8.4 mmol), BHA (2.8 mmol) and olivetol (4.5 mmol) in oxidized linolenic acid [63-65]. After the optimal concentration, a decrease in the antioxidant activity was observed. Interestingly, at high temperatures (<180˚C), the antioxidants are no longer stable and their effectiveness significantly decreased. Similarly, α-tocopherol and L-ascorbic acid 6-palmitate were not effective even at high concentrations (up to 2% wt) during the oxidation of either high oleic sunflower oil or castor oil [66, 69].

6.3. Compensation theory

A proper kinetic interpretation should include the compensation effect, which is usually used to explain whether the variations on effective activation energy values have physical meaning or they are caused by either variations of process conditions or complexity of the reaction systems. In previous investigations [69, 70], the compensation effect is illustrated for various thermal degraded materials, such as polymers, cellulosic materials and CaCO3. The compensation effect can be evaluated by plotting ln k, obtained by equation (7), against 1/T. Figure 9 shows that an increase in the effective activation energy causes an increase in ln k (equation 7). Similarly, a decrease in the effective activation energy results in a lower value of ln k. The point of concurrence, where the different lines intercept, corresponds to ln kiso and 1/Tiso (kiso is the isokinetic rate constant and Tiso is the isokinetic temperature), which indicates the existence of the compensation effect.

Figure 10.

Arrhenius plot (ln k vs 1/T) for the non-isothermal oxidation: (a) compensation effect theory adapted from reference [69], and (b) anhydrous milk fat [9].

In studies of non-isothermal oxidation of anhydrous milk fat (AMF) [9], there is no concurrence at a single point. Therefore, the non-isothermal oxidation of AMF does not exhibit a compensation effect and thus the variations in kinetic parameters have no physical background. In fact, AMF is a very complex fat mainly composed of triacylglycerols that have a glycerol backbone to which three fatty acid moieties are esterified. These triacylglycerols are extremely diverse in chain lengths, position and number of unsaturations of their fatty acids [72]. Moreover, more than 400 fatty acids in milk fat were found [73]. Therefore, several reactions with different constant rates simultaneously occur and DSC only detects those reactions that have the greatest exothermal effect. This could explain why the variations in effective activation energy values have no physical meaning or there is no compensation effect.

The isokinetic temperature can also be defined as the temperature at which two rate constants of two different reactions are equal. For a set of kinetic parameters of two different reactions, the isokinetic temperature can be expressed as:

A1exp(E1RTiso)=A2exp(E2RTiso)E12

The isokinetic temperature of autoxidation of lecithin and linolenic acid calculated using equation (12) was 167˚C [57]. This observation exemplifies the difficulty in determining the oxidative stability of multicomponent systems. For example, if the oxidation test is conducted at a temperature below Tiso, linolenic acid oxidizes faster than lecithin. But, if the same test is conducted at a temperature equal to Tiso, both lipids have the same oxidative stability. Contrary, lecithin oxidizes faster than linolenic acid above Tiso. Consequently, the estimation of the oxidative stability based only on the onset temperature is misleading. Therefore, interpretation of the shape of non-isothermal oxidation curves in combination with kinetic parameters can provide a better interpretation of the oxidative behavior in multicomponent systems.

Advertisement

7. Case studies of lipid oxidation after processing using new technologies

7.1. Kinetics of non-isothermal oxidation of anhydrous milk fat (AMF) rich in conjugated linoleic acid (CLA) after hydrolysis

AMF is the richest source of CLA composed of geometrical and positional isomers of linoleic acid. CLA has potential benefits, such as cancer prevention, atherosclerosis, weight control, and bone formation [74]. Additionally, CLA concentration in milk can be markedly enhanced through diet manipulation and nutritional management of dairy cattle [75]. In CLA-enriched AMF, CLA is distributed throughout different triacylglycerols together with other fatty acids, limiting its applicability as ingredient in different milk fat-based products. One known approach to produce free fatty acids (FFA) is through enzymatic hydrolysis. The enzymatic hydrolysis of AMF rich in CLA yielded around 88% of free fatty acids (FFA) [76, 77]. Unfortunately, FFAs are more susceptible to oxidation than those fatty acids attached to the triacylglycerol backbone.

Figure 10 shows the DSC curves of non-hydrolyzed and hydrolyzed AMF rich in CLA. Although the DSC curves were quite different between non-hydrolyzed AMF (blue and black lines) and hydrolyzed AMF (green and red lines), the maximum peak temperatures were in the same range. This observation supports the hypothesis that changes in the DSC signal below the temperature of the first peak can be attributed to oxidation and changes in DSC signal above TP correspond to thermal decomposition and advanced oxidation products as shown in Figure 8. Figure 10 also shows that the oxidation of hydrolyzed AMF starts at low temperatures (~108˚C), making difficult to obtain a consistent baseline. Therefore, the kinetic parameters were calculated using the onset temperature obtained as described in Section 5.1.

Table 3 shows the onset oxidation temperature and kinetic parameters of non-hydrolyzed and enzymatic hydrolyzed AMF rich in CLA. As expected, the Ea for the hydrolyzed fat is greater than that obtained for the non-hydrolyzed fat. Interestingly, the constant reaction rates (k) calculated at 130 ˚C were similar for the non-hydrolyzed and hydrolyzed samples. However, the constant rate of hydrolyzed fat was dramatically higher than that of non-hydrolyzed fat at 200˚C.

Figure 11.

Non-isothermal oxidation of non-hydrolyzed and hydrolyzed anhydrous milk fat rich in CLA. Tp - maximum heat flow temperature.

Heating rate [˚C/min]Non-hydrolyzed AMF [°C]Hydrolyzed AMF [°C]
3173.47 ± 0.1125.06 ± 1.4
6184.71 ± 2.3132.46 ± 0.3
9192.13 ± 0.7133.25 ± 1.2
12197.85 ± 3.7132.46 ± 0.3
15198.66 ± 0.3136.78 ± 0.1
Ea [kJ/mol]82.42175.78
A [min-1]8.7 x 1072.3 x 1020
k130˚C [min]0.0020.003
k200˚C [min]0.07510.28

Table 3.

Onset temperature of oxidation for anhydrous milk fat (AMF)

The isokinetic temperatures of these two fats were calculated mathematically and graphically using equation (12) and Arrhenius plot, respectively. Figure 11 shows the compensation effect for the oxidation of non-hydrolyzed and hydrolyzed AMF rich in CLA. From this figure, the Tiso and kiso were obtained (Tiso = 120˚C and kiso = 0.0011 min). Similarly, the Tiso and kiso calculated mathematically with equation (12) were 118˚C and 0.0010 min, respectively. However, Tiso for non-hydrolyzed AMF is unrealistic since the start temperature of oxidation is around 155˚C. Therefore, oxidation of either non-hydrolyzed or hydrolyzed AMF rich in CLA does not exhibit a compensation effect.

Figure 12.

Arrhenius plot for the non-isothermal oxidation of non-hydrolyzed and hydrolyzed anhydrous milk fat rich in CLA.

7.2. Oxidative stability of AMF rich in CLA treated with pressure assisted thermal processing

CLA is not stable upon thermal processing and significant losses of its biological activity occurred through oxidation [78]. The application of high pressure (100-600 MPa) to a preheated sample can preserve the biological activity of functional compounds [79]. This is because the rise in temperature due to adiabatic heating is used to reach the target temperature, reducing the thermal damage due to the lack of temperature uniformity that occurs in traditional thermal processes [80, 81]. This technology is known as pressure-assisted thermal processing (PATP). Pressure alters interatomic distance, acting mainly on those weak interactions which bond energy is distance–dependent, such as van der Waals forces, electrostatic forces, hydrogen bonding and hydrophobic interactions of proteins. Based on the distance dependence, any pressurized sample would have its covalent bonds intact. This has been the central hypothesis in preserving the biological activity of functional compounds, such as ascorbic acid, folates, vitamins and anthocyanins [82-85].

The effects of PATP conditions on the antiradical ability of CLA in AMF were reported [86]. CLA can donate hydrogen to form a CLA-free radical that further reacts to inhibit hydroperoxides formation, depending on the final CLA retention. This suggests that the retained CLA after PATP treatment might enhance the oxidative stability of AMF. After PATP treatments, samples of AMF rich in CLA were oxidized at 6˚C/min to calculate the start temperature of oxidation using the method described earlier in Section 5.1 of this chapter.

Figure 12 shows the influence of the retained CLA on the start temperature of oxidation (Ts). The stability of AMF is influenced in a non-linear mode by the CLA retention. Values of the start temperature of oxidation (~165-155˚C) were obtained when the CLA retention was between 85 to 100%. On the other hand, the lowest value of the start temperature of oxidation (141˚C) was obtained at 40% of CLA retention.

Figure 13.

Influence of CLA retention on the start temperature (Ts) of oxidation in anhydrous milk fat rich in CLA.

A possible reason for the CLA-Ts relationship is that CLA can act as an antioxidant capturing those free radicals responsible for the lipid oxidation. This antioxidant behavior was clearly demonstrated in an earlier study by inducing lipid oxidation of fish oil by adding tert-butyl hydroperoxide. CLA effectively reduces lipid peroxidation as measured by chemiluminescence [86]. In addition, the antiradical or scavenging ability of CLA isomers measured by DPPH (2,2-diphenyl-1-picryl-hydrazyl-hydrate) technique depended on the CLA concentration [87].

Advertisement

8. Conclusions

The use of DSC to analyse lipid oxidation is a reliable, simple and convenient technique. It provides qualitative and quantitative information and offers unique advantages, such as the small amount of sample use, short test time, and good reproducibility. Additionally, the effectiveness of a particular antioxidant can be evaluated using DSC, measuring changes in the oxidation onset times or temperatures. The data obtained from DSC lipid oxidation have been extensively studied and correlated with other oxidation methods, such as the Rancimat method, PV, spectrophotometric and GC analysis of fats and oils from various sources.

A proper interpretation of DSC oxidation experiments should include sample composition, kinetic parameters (Ea, A, and k) in combination with the compensation theory. In multicomponent systems, the fat sometimes needs to be extracted from the matrix. Therefore, the lipid oxidative behaviour might be different from its original matrix. The results obtained from DSC oxidation depend upon the conditions used to prepare the sample and the heating protocol used. Factors, such as degree of saturation, amount of free fatty acids, chain length and the presence of natural antioxidants influence the oxidative stability and kinetic parameters. DSC can be coupled with other analytical techniques, such as GC, NMR, HPLC, etc, to provide a better description of the oxidative stability of fats and oils.

Acknowledgement

The authors thank to Alberta Livestock and Meat Agency Ltd. (ALMA) and to the Natural Sciences and Engineering Research Council of Canada (NSERC) for funding this project. Martinez-Monteagudo expresses his gratitude to Consejo Nacional de Ciencia y Tecnologia (CONACYT, Mexico) and Instituto de Inovacion y Transferencia Tecnologica (I2T2, Mexico) for the financial support (nr 187497).

References

  1. 1. Kamal-eldinAPokornJ2005Lipid oxidation products and methods used for their analysis. In Kamal-Eldin A, Pokorny J, editors. Analysis of lipid oxidation. AOCS Publishing, eBook 978-1-43982-239-5
  2. 2. OConnorT. P, OBrienNM (2006Lipid oxidation. In Fox, PF, McSweeney P, editors. Advanced Dairy Chemistry, 2Lipids (3rd Edition). Springer-Verlag. 557600
  3. 3. GrayJ. I1978Measurement of lipid oxidation: A reviewJ. Am. Oil Chem. Soc. 55539546
  4. 4. BradleyD. GMinD. B1992Singlet oxygen of foods. Crit. RevFood Sci. Nutr. 31211236
  5. 5. ShahidiFZhongY2010Lipid oxidation and improving the oxidative stability.Chem. Soc. Rev. 3940674079
  6. 6. LabuzaT. P1971Kinetics of lipid oxidation. Crit. Rev. Food Technol. 2355404
  7. 7. AdhvaryuAErhanS. ZPerezJ. M2000Oxidation kinetic studies of oils derived from unmodified and genetically modified vegetables using pressurized differential scanning calorimetry and nuclear magnetic resonance spectroscopyThermochim. Acta. 3649797
  8. 8. PrivettO. SBlankM. L1962Initial stages of autoxidation. J. Am. Oil Chem. Soc. 39465468
  9. 9. Martínez-monteagudoS. ISaldaña MDA, Kennelly JJ (2012Kinetics of non-isothermal oxidation of anhydrous milk fat rich conjugated linoleic acid using differential scanning calorimetry. JTherm. Anal. Calorim. 107973981
  10. 10. ChoeEMinD. B2006Chemistry and reactions of reactive oxygen species in foodsCrit. Rev. Food Sci. 46122
  11. 11. BrimbergU. IKamal-eldinA2003On the kinetics of the autoxidation of fats substrates with conjugated double bonds.Eur. J. Lipid Sci. Tech. 1051722
  12. 12. HamalainenT. ISundbergSMakkinenMHaseTHopiaA2001Hydroperoxide formation during autoxidation of conjugated linoleic acid methyl esterEur. J. Lipid Sci. Tech. 103588593
  13. 13. KenarJ. AGunstoneF. DKnotheG2007Chapter 8: Chemical properties. In Harwood JL, Frank D, Gunstone FD, Dijkstra AJ, editors. The lipid handbook (3rd Edition). CRC Press. 535590
  14. 14. LopezCLavigneFLesieurPBourgauxCOllivonM2001Thermal and structural behavior of milk fatUnstable species of anhydrous milk fat. J. Dairy Sci. 84756766
  15. 15. JensenR. G2002The composition of bovine milk lipids: January 1995 to December 2000J. Dairy Sci. 85295300
  16. 16. PokornyJ2005Volumetric analysis of oxidized lipids. In Kamal-Eldin A, Pokorny J, editors. Analysis of lipid oxidation. AOCS Publishing.
  17. 17. SimonP2006Induction periods theory and applications. J. Therm. Anal. Calorim. 84263270
  18. 18. FasinaO. OCraig-schmidtMColleyZHallmanH2008Predicting melting characteristics of vegetable oils from fatty acid compositionLWT- Food Sci. Technol. 4115011505
  19. 19. WirkowskaMOstrowska-ligezaEGorskaAKoczonP2012Thermal properties of fats extracted from powdered baby formulasJ. Therm. Anal. Calorim. 110137143
  20. 20. KousksouTJamilAZeraouliYDumasJ. P2006DSC study and computer modelling of the melting process in ice slurryThermochim. Acta. 448123129
  21. 21. CastelloM. LDweckJAranda DAG (2011Kinetic study of thermal processing of glycerol by thermogravimetryJ. Therm. Anal. Calorim. 105737746
  22. 22. RoySRigaA. TAlexanderK. S2002Experimental design aids the development of differential scanning calorimetry standard test procedure for pharmaceuticals.Thermochim. Acta. 392-393:399 EOF
  23. 23. ISO 11357-6:2008 (E) Plastics- differential scanning calorimetry (DSC)- Part 6: Determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT).
  24. 24. TsangWWalkerJ. A1985Characterization of RDF properties through high pressure differential scanning calorimetryResour Conserv. 9355365
  25. 25. AdhvaryuAPerezJ. MSinghI. D1999Application of quantitative NMR spectroscopy to oxidation kinetics of base oils using pressurized differential scanning calorimetry technique.Energ Fuels. 13493498
  26. 26. ButrowA. BSeylerR. J2003Vapor pressure by DSC: extending ASTM E 1782 below 5 kPaThermochim. Acta. 402145152
  27. 27. KousksouTJamilAEl-OmariKZeraouliYLe Guer Y (2011Effect of heating rate and simple geometry on the apparent specific heat capacity: DSC applications. Themochim. Acta. 5195964
  28. 28. LitwinienkoGDanilukAKasprzycka-guttmanT2000Study on autoxidation kinetics of fats by differential scanning calorimetry. 1. Saturated C12C18 fatty acids and their esters. Ind. Eng. Chem. Res. 39:1.12.
  29. 29. VyazovkinSWightC. A1997Kinetics in solids.Annu. Rev. Phys. Chem. 48125149
  30. 30. BouzidiLBoodhooMHumphreyK. LNarineS. S2005Use of the first and second derivatives to accurately determine key parameters of DSC thermographs in lipid crystallization studies. Thermochim. Acta. 43994102
  31. 31. ŠimonP2007The single-step approximation attributes, strong and weak sides.J. Therm. Anal. Calorim. 88709715
  32. 32. VyazovkinSWightC. A1999Model-free and model-fitting approaches to kinetic analysis of isothermal and non-isothermal data. Thermochim. Acta. 3415368
  33. 33. ŠimonPKolmanLNiklovaISchmidtS2000Analysis of the induction period of oxidation of edible oils by differential scanning calorimetryJ. Am. Oil Chem. Soc. 77639642
  34. 34. ŠimonPKolmanL2001DSC study of oxidation induction periodsJ. Therm. Anal. Calorim. 64813820
  35. 35. SchmidMRitterAAffolterS2006Determination of oxidation induction time and temperature by DSCJ. Therm. Anal. Calorim. 2367371
  36. 36. ŠimonPThomasP. SOkuliarJRayA. S2003An incremental integral isoconversional method determination of activation parameters. J. Therm. Anal. Calorim. 72867874
  37. 37. ŠimonPHynekDMalikovaMCibulkovaZ2008Extrapolation of accelerated thermooxidative tests to lower temperatures applying non-Arrhenius temperature functionsJ. Them. Anal. Calorim. 3817821
  38. 38. ŠimonP2009Material stability predictions applying a new non-Arrhenian temperature functionJ. Therm. Anal. Calorim. 2391396
  39. 39. SchmidMAffolterS2003Interlaboratory tests on polymers by differential scanning calorimetry (DSC): determination and comparison of oxidation induction time (OIT) and oxidation induction temperature (OIT*)Polym. Test. 22419428
  40. 40. CrossC. K1970Oil stability: A DSC alternative for the active oxygen methodJ. Amer. Oil Chem. Soc. 47229230
  41. 41. YamazakiMNagaoAKomomiyaK1980High pressure differential thermal analysis of fatty acid methyl esters and triglycerides. J. Amer. Oil Chem. Soc. 575960
  42. 42. RaemyAFroelicherILoeligerJ1987Oxidation of lipids studied by isothermal heat flux calorimetry. Thermochim. Acta. 114159164
  43. 43. ArainSSherazi STH, Bhanger MI, Talpur FN, Mahesar SA (2009Oxidative stability assessment of Bauhinia purpurea seed oil in comparison to tow conventional vegetable oils by differential scanning calorimetry and Rancimat methods. Thermochim. Acta. 48413
  44. 44. Pardauil JJRSouza LKC, Molfetta F, Zamian JR, Filho GNR, da Costa CEF (2011Determination of the oxidative stability by DSC of vegetable oils from the Amazonian areaBioresource Technol. 10258735877
  45. 45. GromodzkaJWardenckiWPawlowiczRMuszynG2010Photoinduced and thermal oxidation of rapeseed and sunflower oils. Eur. J. Lipid Sci. Tech. 11212291235
  46. 46. VelascoJAdersenM. LSkibstedL. H2004Evaluation of oxidative stability of vegetable oils by monitoring the tendency to radical formation. A comparison of electron spin resonance spectroscopy with the Rancimat method and differential scanning calorimetryFood Chem. 85623632
  47. 47. KowalskiB1989Determination of oxidative stability of edible vegetable oils by pressure differential scanning calorimetry. Thermochim. Acta. 156347358
  48. 48. KowalskiBRatuszKMiciulaAKrygierK1997Monitoring of rapeseed oil autoxidation with a pressure differential scanning calorimeterThemochim. Acta. 307177121
  49. 49. RudnikESzczucinskaAGwardiakHSzulcAWiniarskaA2001Comparative studies of oxidative stability of linseed oilThermochim. Acta. 370135140
  50. 50. KowaslkiBRatuszKKowalskaDBekasW2004Determination of the oxidative stability of vegetable oils by differential scanning calorimetry and Rancimat measurements. Eur. J. Lipid Sci. Tech. 106165169
  51. 51. TanC. PChe Man YB, Selamat J, Yusoff MSA (2001Application of Arrhenius kinetics to evaluate oxidative stability in vegetable oils by isothermal differential scanning calorimetry. J. Am. Oil Chem. Soc. 7811331138
  52. 52. TanC. PChe Man YB, Selamat J, Yusoff MSA (2002Comparative studies of oxidative stability of edible oils by differential scanning calorimetry and oxidative stability index methodsFood Chem. 76385389
  53. 53. LitwinienkoGKasprzycka-Guttman, Jarosz-Jarszewska M (1995Dynamic and isothermal DSC investigation of the kinetic of thermooxidative decomposition of some edible oils.J. Therm. Anal. 45741750
  54. 54. LitwinienkiGDanilukaAKasprzycka-guttmanT1999A differential scanning calorimetry study on the oxidation of C12-C18 saturated fatty acids and their esters. J. Am. Oil Chem. Soc. 76655657
  55. 55. CiftiO. NKowalskiBGogusFFadilogluS2009Effect of the addition of a cocoa butter-like fat enzymatically produced from olive pomace oil on the oxidative stability of cocoa butter. J. Food Sci. 4:E184E190.
  56. 56. LitwinienkoG2001Autoxidation of unsaturated fatty acids and their esters. J. Therm. Anal. Calorim. 65639646
  57. 57. LitwinienkoGKasprzycka-guttmanTStudzinskiM1997Effects of selected phenol derivatives on the autoxidation of linolenic acid investigated by DSC non-isothermal methodsThermochim. Acta. 30797106
  58. 58. UlkowskiMMusialikMLitwinienkoG2005Use of differential scanning calorimetry to study lipid oxidation. 1. Oxidative stability of lecithin and linolenic acid.J. Agric. Food. Chem. 5390739077
  59. 59. LitwinienkoGKasprzycka-guttmanT1998A DSC study on thermoxidation kinetics of mustard oilThermochim. Acta. 319185191
  60. 60. Ostrowska-ligezaEBekasWKowalskaDLobaczMWroniakMKowalskiB2010Kinetics of commercial olive oil oxidation: Dynamic differential scanning calorimetry and Rancimat studiesEur. J. Lipid Sci. Tech. 112268274
  61. 61. Jimenez-marquezJBeltran-mazaG2003Aplicación de la calorimetría diferencial de barrido (CDB) en la caracterización del aceite de oliva virgen. Grasas Aceites. 54403409
  62. 62. VittadiniELeeJ. HFregaN. GMinD. BVodovotzY2003DSC determination of thermally oxidized olive oilJ. Am. Oil Chem. Soc. 8533537
  63. 63. ThurgoodJWardRMartiniS2007Oxidation kinetics of soybean oil/anhydrous milk fat blends: A differential scanning calorimetry studyFood Res. Int. 4010301037
  64. 64. LitwinienkoGKasprzycka-guttmanT2000Study on the autoxidation kinetics of fat components by differential scanning calorimetry. 2. Unsaturated fatty acids and their estersInd. Eng. Chem. Res. 391317
  65. 65. PolavkaJPaligovaJCvengrošJŠimonP2005Oxidation stability of methyl esters studied by differential thermal analysis and Rancimat. J. Am. Oil Chem. Soc. 82519524
  66. 66. QuinchiaL. ADelgadoM. AValenciaCFrancoJ. MGallegosC2011Natural and synthetic antioxidant additives for improving the performance of new biolubricant formulationsJ. Agr. Food Chem. 591291712924
  67. 67. KowalskiB1991Thermal-oxidative decomposition of edible oils and fats. DSC stidiesThermochim. Acta. 1844957
  68. 68. MusialikMLitwinienkoG2007DSC study of linolenic acid autoxidation inhibited by BHT, dehydrozingerone and olivetolJ. Therm. Anal. Calorim. 88781785
  69. 69. AgrawalR. K1989The compensation effect- a fact or a fiction. J. Therm. Anal. 35909917
  70. 70. AgrawalR. K1986On the compensation effect. J. Therm. Anal. 317386
  71. 71. LopezCLavigneFLesieurPBourgauxCOllivonM2001Thermal and structural behavior of milk fatUnstable species of anhydrous milk fat. J. Dairy Sci. 84756766
  72. 72. JensenR. G2002The composition of bovine milk lipids: January 1995 to December 2000J. Dairy Sci. 85295300
  73. 73. LockA. LBaumanD. E2004Modifying milk fat composition of dairy cows to enhance fatty acids beneficial to human health.Lipids3911971206
  74. 74. BellJ. AGriinariJ. MKennellyJ. J2006Effect of safflower oil, flaxseed oil, monensin, and vitamin E on concentration of conjugated linoleic acid in bovine milk fat. J. Dairy Sci. 89733748
  75. 75. Martinez-monteagudoS. IKhanMSaldaña MDA, Temelli F (2011Obtaining a milk fraction rich in conjugated linoleic acid. Abstract 45, In 24th Canadian Conference on Fats and Oils, September 2627th, Edmonton, AB, Canada.
  76. 76. Prado GHCKhan M, Saldaña MDA, Temelli F (2012Enzymatic hydrolysis of conjugated linoleic acid-enriched anhydrous milk fat in supercritical carbon dioxideJ. Supercrit. Fluids. 66198206
  77. 77. CampbellWDrakeM. ALarickD. K2003The impact of fortification with conjugated linoleic acid (CLA) on the quality of fluid milk.J. Dairy Sci. 864351
  78. 78. MathysAReinekeKHeinzVKnorrD2009High pressure thermal sterilization- development and application of temperature controlled spore inactivation studies. High Pressure Res. 2937
  79. 79. KnoerzerKBuckowRVersteegC2010Adiabatic compression heating coefficients for high-pressure processing- a study of some insulating polymer materials. J. Food Eng. 98110119
  80. 80. WilsonD. RDabrowskiLStringerSMoezelaarRBrocklehurstT. F2008High pressure in combination with elevated temperature as a method for the sterilization of food. Trends Food Sci. Tech. 19289299
  81. 81. OleyIVerlindePHendrickxMVan LoeyA2006Temperature and pressure stability of L-ascorbic acid and/or [6s] 5-methyltetrahydrofolic acid: A kinetic study. Eur. Food Res. Tech. 2237177
  82. 82. ButzPSerfertYFernandez-garciaADieterichSLindauerRBognarATauscherB2004Influence of high-pressure treatment at 25°C and 80°C on folates in orange juice and model media. J. Food Sci. 69117121
  83. 83. MatserA. AKrebbersBvan den Berg RW, Bartels PV (2004Advantages of high pressure sterilisation on quality of food productsTrends Food Sci. Tech. 157985
  84. 84. VerbeystLOeyIVan Der PlanckenIHendrickxMVan LoeyA2010Kinetic study on the thermal and pressure degradation of anthocyanins in strawberriesFood Chem. 123269274
  85. 85. Martinez-monteagudoS. ISaldaña MDA, Torres JA, Kennelly JJ. (2012Effect of pressure-assisted thermal sterilization on conjugated linoleic acid (CLA) content in CLA-enriched milkInnov Food Sci Emerg Technol, doij.ifset.2012.07.004.
  86. 86. Martinez-monteagudoS. ISaldaña MDA (2011Changes in conjugated linoleic acid (CLA) and antiradical ability of anhydrous milk fat treated with pressure assisted thermal sterilization. Abstract 43, In 24th Canadian Conference on Fats and Oils, September 2627th, Edmonton, AB, Canada.
  87. 87. FagaliNCatalaA2008Antioxidant activity of conjugated acid isomers, linoleic acid and its methyl ester determined by photoemission and DPPH techniques. Biophys.Chem. 1375662

Written By

M.D.A. Saldaña and S.I. Martínez-Monteagudo

Submitted: 20 January 2012 Published: 23 January 2013