Open access

Morphology Characterization of Pitting Corrosion on Sensitized Austenitic Stainless Steel by Digital Image Analysis

Written By

Rosinei Batista Ribeiro, Gilbert Silva, Antônio Henriques Jr. Araujo, Nelson Tavares Matias, José Wilson De Jesus Silva and Bianca Siqueira Martins Domingos

Submitted: 17 September 2013 Published: 20 February 2014

DOI: 10.5772/57256

From the Edited Volume

Developments in Corrosion Protection

Edited by M. Aliofkhazraei

Chapter metrics overview

2,536 Chapter Downloads

View Full Metrics

Written By

Rosinei Batista Ribeiro, Gilbert Silva, Antônio Henriques Jr. Araujo, Nelson Tavares Matias, José Wilson De Jesus Silva and Bianca Siqueira Martins Domingos

Submitted: 17 September 2013 Published: 20 February 2014