Pitting Corrosion Monitoring Using Acoustic Emission

By A. Prateepasen

Submitted: April 16th 2011Reviewed: October 10th 2011Published: March 23rd 2012

DOI: 10.5772/33127

Downloaded: 4678

© 2012 The Author(s). Licensee IntechOpen. This chapter is distributed under the terms of the Creative Commons Attribution 3.0 License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.

How to cite and reference

Link to this chapter Copy to clipboard

Cite this chapter Copy to clipboard

A. Prateepasen (March 23rd 2012). Pitting Corrosion Monitoring Using Acoustic Emission, Pitting Corrosion Nasr Bensalah, IntechOpen, DOI: 10.5772/33127. Available from:

Embed this chapter on your site Copy to clipboard

<iframe src="http://www.intechopen.com/embed/pitting-corrosion/pitting-corrosion-monitoring-using-acoustic-emission" />

Embed this code snippet in the HTML of your website to show this chapter

chapter statistics

4678total chapter downloads

More statistics for editors and authors

Login to your personal dashboard for more detailed statistics on your publications.

Access personal reporting

Related Content

This Book

Next chapter

Oscillatory Phenomena as a Probe to Study Pitting Corrosion of Iron in Halide-Containing Sulfuric Acid Solutions

By Dimitra Sazou, Maria Pavlidou, Aggeliki Diamantopoulou and Michael Pagitsas

Related Book

First chapter

Abrasion Resistance of Polymer Nanocomposites - A Review

By Giulio Malucelli and Francesco Marino

We are IntechOpen, the world's leading publisher of Open Access books. Built by scientists, for scientists. Our readership spans scientists, professors, researchers, librarians, and students, as well as business professionals. We share our knowledge and peer-reveiwed research papers with libraries, scientific and engineering societies, and also work with corporate R&D departments and government entities.

+3,550 Open Access Books

+57,400 Citations in Web of Science

+108,500 IntechOpen Authors and Academic Editors

+560,000 Unique visitors per month

More about us