Oscillatory Phenomena as a Probe to Study Pitting Corrosion of Iron in Halide-Containing Sulfuric Acid Solutions

By Dimitra Sazou, Maria Pavlidou, Aggeliki Diamantopoulou and Michael Pagitsas

Submitted: April 28th 2011Reviewed: September 30th 2011Published: March 23rd 2012

DOI: 10.5772/34202

Downloaded: 2266

© 2012 The Author(s). Licensee IntechOpen. This chapter is distributed under the terms of the Creative Commons Attribution 3.0 License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.

How to cite and reference

Link to this chapter Copy to clipboard

Cite this chapter Copy to clipboard

Dimitra Sazou, Maria Pavlidou, Aggeliki Diamantopoulou and Michael Pagitsas (March 23rd 2012). Oscillatory Phenomena as a Probe to Study Pitting Corrosion of Iron in Halide-Containing Sulfuric Acid Solutions, Pitting Corrosion, Nasr Bensalah, IntechOpen, DOI: 10.5772/34202. Available from:

chapter statistics

2266total chapter downloads

1Crossref citations

More statistics for editors and authors

Login to your personal dashboard for more detailed statistics on your publications.

Access personal reporting

Related Content

This Book

Next chapter

Systemic and Local Tissue Response to Titanium Corrosion

By Daniel Olmedo, Deborah Tasat, Gustavo Duffó, Rómulo Cabrini and María Guglielmotti

Related Book

First chapter

Abrasion Resistance of Polymer Nanocomposites - A Review

By Giulio Malucelli and Francesco Marino

We are IntechOpen, the world's leading publisher of Open Access books. Built by scientists, for scientists. Our readership spans scientists, professors, researchers, librarians, and students, as well as business professionals. We share our knowledge and peer-reveiwed research papers with libraries, scientific and engineering societies, and also work with corporate R&D departments and government entities.

More About Us