Open access peer-reviewed chapter

Corrosive Effects of Chlorides on Metals

By Fong-Yuan Ma

Submitted: April 8th 2011Reviewed: November 7th 2011Published: March 23rd 2012

DOI: 10.5772/32333

Downloaded: 30010

© 2012 The Author(s). Licensee IntechOpen. This chapter is distributed under the terms of the Creative Commons Attribution 3.0 License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.

How to cite and reference

Link to this chapter Copy to clipboard

Cite this chapter Copy to clipboard

Fong-Yuan Ma (March 23rd 2012). Corrosive Effects of Chlorides on Metals, Pitting Corrosion Nasr Bensalah, IntechOpen, DOI: 10.5772/32333. Available from:

Embed this chapter on your site Copy to clipboard

<iframe src="http://www.intechopen.com/embed/pitting-corrosion/corrosive-effects-of-chlorides-on-metals" />

Embed this code snippet in the HTML of your website to show this chapter

chapter statistics

30010total chapter downloads

3Crossref citations

More statistics for editors and authors

Login to your personal dashboard for more detailed statistics on your publications.

Access personal reporting

Related Content

This Book

Next chapter

Electrochemical Characterisation to Study the Pitting Corrosion Behaviour of Beryllium

By J. S. Punni

Related Book

First chapter

Abrasion Resistance of Polymer Nanocomposites - A Review

By Giulio Malucelli and Francesco Marino

We are IntechOpen, the world's leading publisher of Open Access books. Built by scientists, for scientists. Our readership spans scientists, professors, researchers, librarians, and students, as well as business professionals. We share our knowledge and peer-reveiwed research papers with libraries, scientific and engineering societies, and also work with corporate R&D departments and government entities.

+3,550 Open Access Books

+57,400 Citations in Web of Science

+108,500 IntechOpen Authors and Academic Editors

+560,000 Unique visitors per month

More about us