Nanoindentation of Human Trabecular Bone – Tissue Mechanical Properties Compared to Standard Engineering Test Methods

By Ondřej Jiroušek

Submitted: November 24th 2011Reviewed: May 31st 2012Published: October 17th 2012

DOI: 10.5772/50152

Downloaded: 3644

© 2012 The Author(s). Licensee IntechOpen. This chapter is distributed under the terms of the Creative Commons Attribution 3.0 License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.

How to cite and reference

Link to this chapter Copy to clipboard

Cite this chapter Copy to clipboard

Ondřej Jiroušek (October 17th 2012). Nanoindentation of Human Trabecular Bone – Tissue Mechanical Properties Compared to Standard Engineering Test Methods, Nanoindentation in Materials Science, Jiri Nemecek, IntechOpen, DOI: 10.5772/50152. Available from:

chapter statistics

3644total chapter downloads

2Crossref citations

More statistics for editors and authors

Login to your personal dashboard for more detailed statistics on your publications.

Access personal reporting

Related Content

This Book

Next chapter

Design, Analysis and Experiments of a Novel in situ SEM Indentation Device

By Hongwei Zhao, Hu Huang, Zunqiang Fan, Zhaojun Yang and Zhichao Ma

Related Book

First chapter

A Systematic Study and Characterization of Advanced Corrosion Resistance Materials and Their Applications for Plasma Etching Processes in Semiconductor Silicon Wafer Fabrication

By Hong Shih

We are IntechOpen, the world's leading publisher of Open Access books. Built by scientists, for scientists. Our readership spans scientists, professors, researchers, librarians, and students, as well as business professionals. We share our knowledge and peer-reveiwed research papers with libraries, scientific and engineering societies, and also work with corporate R&D departments and government entities.

More About Us