Open access peer-reviewed chapter

Experimental Design and Response Surface Analysis as Available Tools for Statistical Modeling and Optimization of Electrodeposition Processes

By Lilian F. Senna and Aderval S. Luna

Submitted: April 29th 2011Reviewed: October 10th 2011Published: April 11th 2012

DOI: 10.5772/34310

Downloaded: 2385

© 2012 The Author(s). Licensee IntechOpen. This chapter is distributed under the terms of the Creative Commons Attribution 3.0 License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.

How to cite and reference

Link to this chapter Copy to clipboard

Cite this chapter Copy to clipboard

Lilian F. Senna and Aderval S. Luna (April 11th 2012). Experimental Design and Response Surface Analysis as Available Tools for Statistical Modeling and Optimization of Electrodeposition Processes, Electroplating Darwin Sebayang and Sulaiman Bin Haji Hasan, IntechOpen, DOI: 10.5772/34310. Available from:

Embed this chapter on your site Copy to clipboard

<iframe src="http://www.intechopen.com/embed/electroplating/experimental-design-and-response-surface-analysis-as-available-tools-for-statistical-modeling-and-op" />

Embed this code snippet in the HTML of your website to show this chapter

chapter statistics

2385total chapter downloads

More statistics for editors and authors

Login to your personal dashboard for more detailed statistics on your publications.

Access personal reporting

Related Content

This Book

Next chapter

Preparation of NiO Catalyst on FeCrAl Substrate Using Various Techniques at Higher Oxidation Process

By Darwin Sebayang, Yanuandri Putrasari, Sulaiman Hasan, Mohd Ashraf Othman and Pudji Untoro

Related Book

First chapter

Principle Operation of 3-D Memory Device based on Piezoacousto Properties of Ferroelectric Films

By Ju. H. Krieger

We are IntechOpen, the world's leading publisher of Open Access books. Built by scientists, for scientists. Our readership spans scientists, professors, researchers, librarians, and students, as well as business professionals. We share our knowledge and peer-reveiwed research papers with libraries, scientific and engineering societies, and also work with corporate R&D departments and government entities.

+3,550 Open Access Books

+57,400 Citations in Web of Science

+108,500 IntechOpen Authors and Academic Editors

+560,000 Unique visitors per month

More about us