Assessment of Stress Corrosion Cracking on Pipeline Steels Weldments Used in the Petroleum Industry by Slow Strain Rate Tests

By A. Contreras, M. Salazar, A. Albiter, R. Galván and O. Vega

Submitted: February 9th 2011Reviewed: July 22nd 2011Published: December 16th 2011

DOI: 10.5772/26569

Downloaded: 12282

© 2011 The Author(s). Licensee IntechOpen. This chapter is distributed under the terms of the Creative Commons Attribution 3.0 License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.

How to cite and reference

Link to this chapter Copy to clipboard

Cite this chapter Copy to clipboard

A. Contreras, M. Salazar, A. Albiter, R. Galván and O. Vega (December 16th 2011). Assessment of Stress Corrosion Cracking on Pipeline Steels Weldments Used in the Petroleum Industry by Slow Strain Rate Tests, Arc Welding Wladislav Sudnik, IntechOpen, DOI: 10.5772/26569. Available from:

Embed this chapter on your site Copy to clipboard

<iframe src="http://www.intechopen.com/embed/arc-welding/assessment-of-stress-corrosion-cracking-on-pipeline-steels-weldments-used-in-the-petroleum-industry-" />

Embed this code snippet in the HTML of your website to show this chapter

chapter statistics

12282total chapter downloads

1Crossref citations

More statistics for editors and authors

Login to your personal dashboard for more detailed statistics on your publications.

Access personal reporting

Related Content

This Book

Next chapter

Evaluation of the Shielding Gas Influence on the Weldability of Ferritic Stainless Steel

By Demostenes Ferreira Filho, Ruham Pablo Reis and Valtair Antonio Ferraresi

Related Book

First chapter

Mechanical Transmissions Parameter Modelling

By Isad Saric, Nedzad Repcic and Adil Muminovic

We are IntechOpen, the world's leading publisher of Open Access books. Built by scientists, for scientists. Our readership spans scientists, professors, researchers, librarians, and students, as well as business professionals. We share our knowledge and peer-reveiwed research papers with libraries, scientific and engineering societies, and also work with corporate R&D departments and government entities.

+3,550 Open Access Books

+57,400 Citations in Web of Science

+108,500 IntechOpen Authors and Academic Editors

+560,000 Unique visitors per month

More about us