Experimental Design and Response Surface Analysis as Available Tools for Statistical Modeling and Optimization of Electrodeposition Processes

Written By

Lilian F. Senna and Aderval S. Luna

Submitted: 29 April 2011 Published: 11 April 2012

DOI: 10.5772/34310

From the Edited Volume

Electroplating

Edited by Darwin Sebayang and Sulaiman Bin Haji Hasan